Cleaning and post-treatment
After silver plating, the following steps are performed in sequence:
1. Three rinses with deionized water to remove free silver ions
2. Two washes with ethanol to remove organic residues
3. Vacuum drying oven at 80℃ for constant temperature dehydration
4. Sieve and classify (200-400 mesh)
Performance improvement
By optimizing the protective agent combination scheme (gelatin and polyvinylpyrrolidone compound), the uniformity of silver layer thickness is improved by more than 20% . The improved glass powder exhibits the following in conductive silver paste:
Contact resistance is reduced to below 0.5Ω·cm
Silver layer adhesion reaches 5B grade (ASTM D3359 standard)
No silver layer peeling after high-temperature sintering